92-6040 Series
Manufacturer: Kester Solder
SOLDER FLUX-CORED/245 .025" 500G
| Part | Composition | Flux Type | Wire Gauge | Process | Form | Form | Form | Type | Storage/Refrigeration Temperature [Max] | Storage/Refrigeration Temperature [Min] | Wire Gauge | Diameter [diameter] | Diameter [diameter] |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Kester Solder | Sn60Pb40 (60/40) | No-Clean | 30 AWG 33 SWG | Leaded | 17.64 oz | Spool | 500 g | Wire Solder | 40 °C 104 F | 10 C 50 F | |||
Kester Solder | Sn60Pb40 (60/40) | No-Clean | Leaded | 17.64 oz | Spool | 500 g | Wire Solder | 40 °C 104 F | 10 C 50 F | 20 AWG 22 SWG | |||
Kester Solder | Sn60Pb40 (60/40) | Rosin Activated (RA) | Leaded | 17.64 oz | Spool | 500 g | Wire Solder | 40 °C 104 F | 10 C 50 F | 20 AWG 22 SWG | |||
Kester Solder | Sn60Pb40 (60/40) | Rosin Activated (RA) | Leaded | 17.64 oz | Spool | 500 g | Wire Solder | 40 °C 104 F | 10 C 50 F | 22 AWG 23 SWG | |||
Kester Solder | Sn60Pb40 (60/40) | Rosin Activated (RA) | Leaded | 17.64 oz | Spool | 500 g | Wire Solder | 40 °C 104 F | 10 C 50 F | 20 AWG 22 SWG | |||
Kester Solder | Sn60Pb40 (60/40) | No-Clean | Leaded | 17.64 oz | Spool | 500 g | Wire Solder | 40 °C 104 F | 10 C 50 F | 20 AWG 22 SWG | |||
Kester Solder | Sn60Pb40 (60/40) | No-Clean | 18 19 | Leaded | 17.64 oz | Spool | 500 g | Wire Solder | 40 °C 104 F | 10 C 50 F | 1.02 mm | 0.04 in |